Abstract:
A two-step process for the fabrication of 0.12-1.20- mu m-thick Tl/sub 2/Ba/sub 2/CaCu/sub 2/O/sub 8/ films onMetadata
Abstract:
A two-step process for the fabrication of 0.12-1.20- mu m-thick Tl/sub 2/Ba/sub 2/CaCu/sub 2/O/sub 8/ films on
Published in: IEEE Transactions on Magnetics ( Volume: 27, Issue: 2, March 1991)
DOI: 10.1109/20.133982